NPP-688-C transparent rubber paste mixed with NPP-688-W white rubber paste and BCA-3070 Bottoming Additive 1% to bottom the basis twice.
|
◇
|
Mix up NPP-688-CKC with NPP-688-CKW by 50~70% and 50~30%, respectively to print.
|
◇
|
Printing operation can be performed after slightly dried for the next layer.
|
◇
|
The more percentage of NPP-688-CKC applied the more strength of downward- binding gained.
|
◇
|
Mixing with PRC series is highly recommended to produce accurate
|
|
and bright colors.
|
◇
|
Suitable for screen with less 120 mesh.
|